Valorizing Duck Bone into Regenerable Hydroxyapatite Biochar: Pyrolysis Effects on Divalent Heavy Metal Adsorption Mechanisms.
Hongthong Sukanya S, Kreethachat Torpong T, Imman Saksit S, Suriyachai Nopparat N et al.
Duck bone, an under-used by-product of Southeast Asian poultry processing, was converted into hydroxyapatite-based bone char by single-step, reagent-free pyrolysis at 300, 400, and 500 °C and evaluated as a reusable Cu(II) adsorbent. Physical and chemical analyses showed progressive removal of the collagen-lipid matrix and preservation of a hydroxyapatite scaffold (98-99 wt% of the crystalline phases by Rietveld refinement, with minor calcite; apparent crystallite size ~7-8 nm across and ~23-25 nm along the c-axis). Surface area increased progressively from 33.0 to 84.2 m2 g-1 with pyrolysis temperature, whereas the Toth capacity increased steadily from 44.7 to 48.6 mg g-1, indicating that uptake is governed mainly by apatite-site accessibility rather than scaling proportionally with surface area. Sigmoidal Avrami kinetics with exponents of 1.25-1.48, sharply saturating isotherms, an endothermic enthalpy of 71-90 kJ mol-1, and points of zero charge of about pH 7-9.5 supported cooperative binding through Ca2+-Cu2+ ion exchange, phosphate and hydroxyl complexation, and proposed surface nucleation of Cu-phosphate clusters; Cu(OH)2 precipitation was not expected at the pH used. After five HCl regeneration cycles, DKB retained 73.1-80.0% of its initial efficiency, and the first-order decay constant decreased from 0.078 to 0.056 cycle-1 with increasing pyrolysis temperature. DKB produced at 500 °C combined the highest capacity, fastest kinetics, and greatest regeneration stability, establishing duck bone as a low-cost, circular feedstock for Cu(II) remediation.